Extract

"The deposition was followed by drying for 45 min at 50 °C in a vacuum. The next step was photopolymerization under UV light (365 nm from CoolLED pE-4000 focused on sample area), the time required for complete cross-linking of PNIPAm-BP-RhB copolymer was 40 min. "